Polypropylene with 30% glass fiber content is resistant to concentrated solutions of acids and alkalis.
It is recommended to print on regular polypropylene tape as a table cover (in this case there is no need to heat the printing table), OR heat the table to 60-70C and use a rough coating (the back of a mirror, ceramics, frosted glass, etc.), border in In this case (Brim) will also not hurt when slicing.
Printing options
- Nozzle temperature 235-255°C
- Print bed temperature 0-60°C
- Blowing the model as needed up to 50%
- Printing speed 30-50 mm/s
- Plastic supply (Flow) 100-105%
- Nozzle diameter from 0.4 mm (min)
- Min. layer height 0.15 mm
- Bending temperature under load (1.8 MPa) +145°С
- Charpy impact strength without notch (+23°C) 46 kJ/m2
- Charpy impact strength without notch (-45°C) 20 kJ/m2
- Tolerance on rod diameter 0.03 mm
- Quantity on reel ~ 280 m
- Shrinkage 0.5%
- Hardness Shore A —
- Elongation at break 4%
- Maximum tensile strength 75 MPa
- Density ~1.15 g/cm3
Reviews
There are no reviews yet.